CN208811086U - A kind of long nozzle mold for forming of hard alloy type - Google Patents
A kind of long nozzle mold for forming of hard alloy type Download PDFInfo
- Publication number
- CN208811086U CN208811086U CN201821579855.4U CN201821579855U CN208811086U CN 208811086 U CN208811086 U CN 208811086U CN 201821579855 U CN201821579855 U CN 201821579855U CN 208811086 U CN208811086 U CN 208811086U
- Authority
- CN
- China
- Prior art keywords
- prod cast
- mold
- nut
- core
- retainer plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The utility model discloses a kind of long nozzle mold for forming of hard alloy type, it is characterized in that, including housing, one end is equipped with first end blocking piece in the housing, and the inner end of the first end blocking piece is equipped with mold core, is cased with prod cast core retainer plate on the other end of the mold core, nut is equipped at one end medium position of the prod cast core retainer plate, the nut is threaded on mold core, and the other end of the prod cast core retainer plate is stifled equipped with second end, and it is stifled interior that the nut is located at second end;The utility model structure is simple, can be realized basic green compact operation, further, can suppress and obtain strong green compact, and facilitate and be removed from the molds green compact, have stronger practicability.
Description
Technical field
The utility model relates to casting-sinter process mould therefor correlative technology field more particularly to a kind of hard alloy type are long
Nozzle mold for forming.
Background technique
Casting-sinter process combines the feature of casting technique, powder metallurgy, self-propagating high-temperature, mainly for the preparation of Metal Substrate
Composite material.It is damaged by pressure, composite material green compact on the basis of traditional casting technique in cast(ing) surface layer composite layer composite material
Under the action of high-temperature liquid metal, high-temperature chemical reaction, a large amount of ceramic particle of in-situ preparation, TiC, VC etc. occurs.It is in situ anti-
The generation answered, so that composite layer has extremely superior performance, to extend the service life of metal material.
The process flow of casting-sinter process is as follows:
First according to alloyage powder is required, then on press by powder pressing at the green compact with higher density,
Green compact is placed in the casting mold prepared again, finally pours molten metal in people's casting mold.After metal freezing, composite material green compact
It completes around knot and densification process, and metallurgical bonding occurs with casting parent and is integrally formed.It is adopted according to the design feature of workpiece
With the method, surface composite layer can be prepared with a thickness of the workpiece of 3-10mm.In entire forming process, along with following
The progress and completion of process.
1. composite wood section damages by pressure under the action of high-temperature liquid metal, high-temperature chemical reaction occurs, in-situ preparation is largely made pottery
Porcelain particle.Such as TC, VC, reaction in-situ make composite layer with extremely superior performance, e.g., resistance to the making property of high wearability,
Southern high temperature oxidation stability etc..Composite material damages the process that in-situ chemical reaction is completed under high-temperature liquid metal excitation, essential table by pressure
Reveal the feature of conbustion synthesis.During such a, phenomena such as including igniting to composite layer, the transmitting of combustion wave.
Here it is the self- propagating features of casting-sinter process.
2. composite wood section green compact under the action of high-temperature liquid metal, occurs sintering and political affairs densification, makes composite layer
With meeting structure feature required by substrate performance.Burning when prepared by this sintering and densification process and powdered metallurgical material
Knot and densification process are much like.This is the powder metallurgy feature of casting-sinter process.
3. under the action of high-temperature liquid metal, the metallurgical bonding between casting parent occurs for composite material green compact, so that
Composite layer becomes organic whole after casting solidification completion, with casting.Such metallurgical bonding, so that composite material
Layer is under the conditions of bearing huge alternating load, and under high thermal shock, the peeling conditions with parent will not occur.Together
When, the forming of casting body is disposably completed in a manner of liquid forming, this makes casting-sinter process show distinct casting
Feature.And if long nozzle as described in Figure 1 is cast using casting-sinter process, it can be seen from the figure that this each portion of long nozzle
There is differences for the wall thickness and diameter of position, and the green compact for the long nozzle of hard alloy type proposes biggish challenge, if adopting
It with traditional mold and is easy to appear, alloy powder the phenomenon that alloy powder is not compacted occurs in the process of compacting, and demoulding is tired
Difficulty greatly may generate damage to green compact during demoulding, therefore design and a kind of be able to solve the special of above-mentioned technical problem
It is very urgent with mold.
Utility model content
The utility model provides a kind of long nozzle mold for forming of hard alloy type, to solve the above-mentioned prior art not
Foot can be realized basic green compact operation, further, can suppress and obtain strong green compact, and facilitate green compact from mold
Middle taking-up has stronger practicability.
In order to realize the purpose of this utility model, the following technology of proposed adoption:
A kind of long nozzle mold for forming of hard alloy type, which is characterized in that including housing, one end is equipped in the housing
First end blocking piece, the inner end of the first end blocking piece are equipped with mold core, are cased with prod cast core retainer plate, institute on the other end of the mold core
It states and is equipped with nut at one end medium position of prod cast core retainer plate, the nut is threaded on mold core, on the other end of the prod cast core retainer plate
Stifled equipped with second end, it is stifled interior that the nut is located at second end;
Described jacket internal one end is equipped with one section of straight die cavity, and the first end blocking piece is set to the outboard end in straight die cavity, institute
The other end for stating straight die cavity is equipped with prod cast chamber, and the prod cast core retainer plate is set at prod cast chamber, sets on the other end of the prod cast chamber
There is covering chamber, the second end is stifled intracavitary set on covering;
First end blocking piece one end is equipped with circular hole;
The mold core includes assembly, and the assembly is set in circular hole, and one end of the assembly is equipped with prod cast
Core bar, the other end of the prod cast core bar are equipped with straight core rod, and the other end of the straight core rod is equipped with assembling bar, described
Prod cast core bar and straight core rod are located in straight die cavity;
One end of the prod cast core retainer plate is equipped with matrix, and one end of the matrix is equipped with cone block, the cone block and matrix
Through there is assembly hole, the assembling bar is through in assembly hole center position, and the nut is set on the bared end of assembling bar;
Matrix assembly hole and nut bore are equipped in the second end is stifled, the matrix is set in matrix assembly hole, the spiral shell
Mother is located in nut bore.
Preferably, the end of the assembly is equipped with collar extension.
Preferably, the outboard end side wall of the first end blocking piece is equipped with the first arc ring.
Preferably, the stifled outboard end side wall of the second end is equipped with the second arc ring.
Preferably, the diameter of the covering chamber is greater than the diameter of straight die cavity.
Preferably, the housing rubber is made.
The advantages of above-mentioned technical proposal, is:
1, housing, first end blocking piece, mold core, prod cast core retainer plate, nut and the second end being equipped with according to the utility model are blocked up,
By being used cooperatively for above several different components, the green compact that can suppress as shown in Fig. 1, wherein rubber sleeve can
Effectively the pressure that the external world provides is transmitted on alloy powder, so that alloy powder is suppressed into corresponding green compact;First
End blocking piece and second end are blocked up and can be prevented when suppressing alloy powder, and alloy powder therefrom sprays;Mold core, prod cast core retainer plate and spiral shell
Mother, the long nozzle interior shape that the mutual cooperation of three can be suppressed as shown in Fig. 1, wherein nut is by mold core and prod cast
Core retainer plate is stable to be combined;
2, the first arc ring and the second arc ring being equipped with are blocked according to first end blocking piece in the utility model and second end
The air in housing can be facilitated to be discharged when squeezing alloy powder, to effectively prevent green compact from stomata occur, thus shadow
Ring the quality of long nozzle;Secondly when constantly externally set is squeezed, first end blocking piece and second end are stifled can be tight with housing
Combination, to effectively prevent alloy powder from washing open under excessive pressure by first end blocking piece and second end are stifled;
3, the collar extension being equipped with according to the end of assembly in the utility model, can accommodate a small amount of air, thus first
End blocking piece and second end is stifled tightly combined with housing after, provide a cavity for the discharge of the air in alloy powder;
4, the utility model structure is simple, can be realized basic green compact operation, further, can suppress obtain it is strong
Green compact, and facilitate and be removed from the molds green compact, there is stronger practicability.
Detailed description of the invention
Fig. 1 shows long nozzle section figure.
Fig. 2 shows the utility model entirety sectional views.
Fig. 3 shows housing sectional axonometric drawing.
Fig. 4 shows first end blocking piece three-dimensional structure diagram.
Fig. 5 shows mold core three-dimensional structure diagram.
Fig. 6 shows prod cast core retainer plate three-dimensional structure diagram.
Fig. 7 shows second end and blocks up three-dimensional structure diagram.
Specific embodiment
It is practical to this below in conjunction with attached drawing in order to keep the purpose of this utility model, technical solution and advantage clearer
It is novel to be described in further detail.
As shown in Fig. 1-Fig. 7, a kind of long nozzle mold for forming of hard alloy type, which is characterized in that including housing 1, institute
State in housing 1 one end and be equipped with first end blocking piece 2, the inner end of the first end blocking piece 2 is equipped with mold core 3, the mold core 3 it is another
It is cased with prod cast core retainer plate 4 on one end, is equipped with nut 5 at one end medium position of the prod cast core retainer plate 4, the nut 5 is threaded onto mold core 3
On, the other end of the prod cast core retainer plate 4 is equipped with second end stifled 6, and the nut 5 is located in second end stifled 6;
Described 1 inside one end of housing is equipped with 10 1 sections of straight die cavity, and the first end blocking piece 2 is set to the outside in straight die cavity 10
End, the other end of the straight die cavity 10 are equipped with prod cast chamber 11, and the prod cast core retainer plate 4 is set at prod cast chamber 11, the prod cast chamber
11 other end is equipped with covering chamber 12, and the second end stifled 6 is set in covering chamber 12;
Described 2 one end of first end blocking piece is equipped with circular hole 21;
The mold core 3 includes assembly 30, and the assembly 30 is set in circular hole 21, on one end of the assembly 30
Equipped with prod cast core bar 31, the other end of the prod cast core bar 31 is equipped with straight core rod 32, the other end of the straight core rod 32
It is equipped with assembling bar 33, the prod cast core bar 31 and straight core rod 32 are located in straight die cavity 10;
One end of the prod cast core retainer plate 4 is equipped with matrix 40, and one end of the matrix 40 is equipped with cone block 41, the cone block 41
Through there is assembly hole 42, the assembling bar 33 is through in assembly hole 42 center position with matrix 40, and the nut 5 is set to group
On the bared end for filling bar 33;
Matrix assembly hole 61 and nut bore 62 are equipped in the second end stifled 6, the matrix 40 is set to matrix assembly hole 61
Interior, the nut 5 is located in nut bore 62.
Preferably, the end of the assembly 30 is equipped with collar extension 300.
Preferably, the outboard end side wall of the first end blocking piece 2 is equipped with the first arc ring 20.
Preferably, the outboard end side wall of the second end stifled 6 is equipped with the second arc ring 60.
Preferably, the diameter of the covering chamber 12 is greater than the diameter of straight die cavity 10.
Preferably, 1 rubber of housing is made.
The utility model specific embodiment is as described below:
Mold core 3 is through in housing 1 by one, and to ensure that prod cast core bar 31 and straight core rod 32 are located in straight die cavity 10;
First end blocking piece 2 is assemblied on one end of straight die cavity 10 by two, and to ensure that assembly 30 is assemblied in circular hole 21
It is interior;
Prod cast core retainer plate 4 is assemblied on assembling bar 33 by three, and prod cast core retainer plate 4 is tightened in assembling bar 33 using nut 5
On;
Four, are packed into the alloy powder of sufficient amount into housing 1;
Second end is blocked up 6 and is assemblied in covering chamber 12 by five, and ensures that nut 5 is located in nut bore 62;
Six, come into effect compacting;
After the completion of seven, compacting, second end stifled 6 is first extracted, nut 5 is then unclamped, prod cast core retainer plate 4 is extracted, is then extracted
First end blocking piece 2 then extracts mold core 3, finally takes out green compact, and compacting is completed.
The above is only the preferred embodiment of the present invention, is not intended to limit the utility model, it is clear that this field
Technical staff various modification and variations can be carried out to the utility model without departing from the spirit and scope of the utility model.This
Sample, if these modifications and variations of the present invention belong to the claims of the present invention and its equivalent technology range it
Interior, then the utility model is also intended to include these modifications and variations.
Claims (6)
1. a kind of long nozzle mold for forming of hard alloy type, which is characterized in that including housing (1), the interior one end of the housing (1)
Equipped with first end blocking piece (2), the inner end of the first end blocking piece (2) is equipped with mold core (3), the other end of the mold core (3)
On be cased with prod cast core retainer plate (4), be equipped with nut (5) at one end medium position of the prod cast core retainer plate (4), the nut (5) is threaded onto
On mold core (3), the other end of the prod cast core retainer plate (4) is equipped with second end and blocks up (6), and the nut (5) is located at second end and blocks up (6)
It is interior;
The internal one end of the housing (1) is equipped with (10) one sections of straight die cavity, and the first end blocking piece (2) is set in straight die cavity (10)
The other end of outboard end, the straight die cavity (10) is equipped with prod cast chamber (11), and the prod cast core retainer plate (4) is set to prod cast chamber (11)
The other end at place, the prod cast chamber (11) is equipped with covering chamber (12), and the second end is blocked up (6) and is set in covering chamber (12);
Described first end blocking piece (2) one end is equipped with circular hole (21);
The mold core (3) includes assembly (30), and the assembly (30) is set in circular hole (21), the assembly (30)
One end is equipped with prod cast core bar (31), and the other end of the prod cast core bar (31) is equipped with straight core rod (32), the straight mold core
The other end of bar (32) is equipped with assembling bar (33), and the prod cast core bar (31) and straight core rod (32) are located at straight die cavity (10)
It is interior;
One end of the prod cast core retainer plate (4) is equipped with matrix (40), and one end of the matrix (40) is equipped with cone block (41), the cone
Through there is assembly hole (42), the assembling bar (33) is through in assembly hole (42) center position of block (41) and matrix (40),
The nut (5) is set on the bared end of assembling bar (33);
The second end blocks up and is equipped with matrix assembly hole (61) and nut bore (62) in (6), and the matrix (40) assembles set on matrix
In hole (61), the nut (5) is located in nut bore (62).
2. the long nozzle mold for forming of hard alloy type according to claim 1, which is characterized in that the assembly (30)
End be equipped with collar extension (300).
3. the long nozzle mold for forming of hard alloy type according to claim 1, which is characterized in that the first end blocking piece
(2) outboard end side wall is equipped with the first arc ring (20).
4. the long nozzle mold for forming of hard alloy type according to claim 1, which is characterized in that the second end is stifled
(6) outboard end side wall is equipped with the second arc ring (60).
5. the long nozzle mold for forming of hard alloy type according to claim 1, which is characterized in that the covering chamber (12)
Diameter be greater than straight die cavity (10) diameter.
6. the long nozzle mold for forming of hard alloy type according to claim 1, which is characterized in that housing (1) rubber
Glue is made.