CN105751534A - 一种大型传送带的粘接修复工艺 - Google Patents

一种大型传送带的粘接修复工艺 Download PDF

Info

Publication number
CN105751534A
CN105751534A CN201410761271.9A CN201410761271A CN105751534A CN 105751534 A CN105751534 A CN 105751534A CN 201410761271 A CN201410761271 A CN 201410761271A CN 105751534 A CN105751534 A CN 105751534A
Authority
CN
China
Prior art keywords
adhesive
joint
layer
bonding
neoprene
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410761271.9A
Other languages
English (en)
Inventor
张翠云
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chongqing Huande Technology Co Ltd
Original Assignee
Chongqing Huande Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chongqing Huande Technology Co Ltd filed Critical Chongqing Huande Technology Co Ltd
Priority to CN201410761271.9A priority Critical patent/CN105751534A/zh
Publication of CN105751534A publication Critical patent/CN105751534A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种大型传送带的粘接修复工艺,包括如下步骤,1)胶黏剂选择:维修时传送带选用氯丁胶粘剂并补充列克纳作胶黏剂;2)料补工艺:① 表面处理 将脱胶部位全部撕开,用钢丝打磨机把老化橡胶层全部磨掉,使之露山新衅表面,先用汽油清洗数遍,最后用甲苯清洗2遍,晾干;②配胶 将氯丁胶与列克纳按比例调和均匀;③ 粘接 用毛刷在2被粘表面分别涂一层胶,厚约0.2mm,晾置5min后再涂第2遍;④ 固化 用大于接头尺寸的两钢板夹紧接头,并用螺栓紧固,压力约为0.5MPa,常温固化30h;⑤ 为了防止接头处经过传动辊时磨擦起皮,再在接头处粘一层棉质细帆布保护。

Description

一种大型传送带的粘接修复工艺
技术领域
本发明涉及一种大型传送带的粘接修复工艺。
背景技术
传送带是输送零件或者货物的重要部件,由于长时间处于载荷状态,所以易出现磨损断裂的现象,所以需要进行修复,目前的修复工艺而其工序安排不合理、工序繁多,时间长,已经不能满足要求,需要加以改进以提高性能。发明内容
有鉴于现有技术的上述缺陷,本发明所要解决的技术问题是提供一种大型传送带的粘结修复工艺,该修复工艺方法简单,能快速修复传送带,增加其使用寿命,减低成本。
为实现上述目的,本发明提供了一种大型传送带的粘接修复工艺,其特征在于,包括如下步骤,1)胶黏剂选择:维修时传送带选用氯丁胶粘剂并补充列克纳作胶黏剂,氯丁胶与列克纳质量比为100:10。
2)料补工艺
  ① 表面处理 将脱胶部位全部撕开,用钢丝打磨机把老化橡胶层全部磨掉,使之露山新衅表面,先用汽油清洗数遍,最后用甲苯清洗2遍,晾干;
  ② 配胶 将氯丁胶与列克纳按比例调和均匀;
  ③ 粘接 用毛刷在2被粘表面分别涂一层胶,厚约0.2mm,晾置5min后再涂第2遍,当胶层晾置至不粘手时,从中间往外一次合拢粘接,用榔头从中间往外敲击赶掉气泡;
  ④ 固化 用大于接头尺寸的两钢板夹紧接头,并用螺栓紧固,压力约为0.5MPa,常温固化30h;
  ⑤ 为了防止接头处经过传动辊时磨擦起皮,再在接头处粘一层棉质细帆布保护。
本发明的有益效果是:本发明工艺方法简单,能快速修复传送带,增加其使用寿命,减低成本。
具体实施方式
本发明公开的技术方案是一种大型传送带的粘接修复工艺,其特征在于,包括如下步骤,1)胶黏剂选择:维修时传送带选用氯丁胶粘剂并补充列克纳作胶黏剂,氯丁胶与列克纳质量比为100:10。
2)料补工艺
  ① 表面处理 将脱胶部位全部撕开,用钢丝打磨机把老化橡胶层全部磨掉,使之露山新衅表面,先用汽油清洗数遍,最后用甲苯清洗2遍,晾干;
  ② 配胶 将氯丁胶与列克纳按比例调和均匀;
  ③ 粘接 用毛刷在2被粘表面分别涂一层胶,厚约0.2mm,晾置5min后再涂第2遍,当胶层晾置至不粘手时,从中间往外一次合拢粘接,用榔头从中间往外敲击赶掉气泡;
  ④ 固化 用大于接头尺寸的两钢板夹紧接头,并用螺栓紧固,压力约为0.5MPa,常温固化30h;
  ⑤ 为了防止接头处经过传动辊时磨擦起皮,再在接头处粘一层棉质细帆布保护。
本发明工艺方法简单,能快速修复传送带,增加其使用寿命,减低成本。
以上详细描述了本发明的较佳具体实施例。应当理解,本领域的普通技术人员无需创造性劳动就可以根据本发明的构思作出诸多修改和变化。因此,凡本技术领域中技术人员依本发明的构思在现有技术的基础上通过逻辑分析、推理或者有限的实验可以得到的技术方案,皆应在由权利要求书所确定的保护范围内。

Claims (1)

1.一种大型传送带的粘接修复工艺,其特征在于,包括如下步骤,1)胶黏剂选择:维修时传送带选用氯丁胶粘剂并补充列克纳作胶黏剂,氯丁胶与列克纳质量比为100:10;
2)料补工艺
  ① 表面处理 将脱胶部位全部撕开,用钢丝打磨机把老化橡胶层全部磨掉,使之露山新衅表面,先用汽油清洗数遍,最后用甲苯清洗2遍,晾干;
  ② 配胶 将氯丁胶与列克纳按比例调和均匀;
  ③ 粘接 用毛刷在2被粘表面分别涂一层胶,厚约0.2mm,晾置5min后再涂第2遍,当胶层晾置至不粘手时,从中间往外一次合拢粘接,用榔头从中间往外敲击赶掉气泡;
  ④ 固化 用大于接头尺寸的两钢板夹紧接头,并用螺栓紧固,压力约为0.5MPa,常温固化30h;
  ⑤ 为了防止接头处经过传动辊时磨擦起皮,再在接头处粘一层棉质细帆布保护。
CN201410761271.9A 2014-12-13 2014-12-13 一种大型传送带的粘接修复工艺 Pending CN105751534A (zh)