JPS5528554A - Magnetic recording medium - Google Patents
Magnetic recording mediumInfo
- Publication number
- JPS5528554A JPS5528554A JP10124778A JP10124778A JPS5528554A JP S5528554 A JPS5528554 A JP S5528554A JP 10124778 A JP10124778 A JP 10124778A JP 10124778 A JP10124778 A JP 10124778A JP S5528554 A JPS5528554 A JP S5528554A
- Authority
- JP
- Japan
- Prior art keywords
- magnetic
- powder
- lubricant
- magnetic layer
- perphloro
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To increase the wearing properties by mixing the perphloro alkyl polyether and the prescribed aliphatic alcohol as the lubricant into the magnetic layer.
CONSTITUTION: The magnetic coating material composed of the magnetic powder and the binding agent is coated on the substrate such as the polyester film or the like to form the magnetic layer and then to obtain the magnetic tape and the like. Then the double-component system lubricant featuring, for example, 70:30W99.5:0.5 weight ratio between the perphloro polyether and the aliphatic alcohol of the carbon number 12W20 is mixed into the magnetic layer of the above mentioned magnetic tape. The wearing properties can be enhanced more by using the nonmagnetic powder featuring the Mohs' hardness of over 6 together. The quantity of the lubricant to be used is set preferably to 1W25 part by weight to 100 of the magnetic powder, and the nonmagnetic powder is set to 0.5W5wt% to the magnetic powder respectively.
COPYRIGHT: (C)1980,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10124778A JPS5528554A (en) | 1978-08-19 | 1978-08-19 | Magnetic recording medium |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP10124778A JPS5528554A (en) | 1978-08-19 | 1978-08-19 | Magnetic recording medium |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5528554A true JPS5528554A (en) | 1980-02-29 |
Family
ID=14295567
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP10124778A Pending JPS5528554A (en) | 1978-08-19 | 1978-08-19 | Magnetic recording medium |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5528554A (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS59107428A (en) * | 1982-12-10 | 1984-06-21 | Seiko Epson Corp | Formation of lubricating layer for magnetic recording medium |
US7624496B2 (en) * | 2003-08-29 | 2009-12-01 | Hitachi Global Storage Technologies Netherlands B.V. | Method for efficient slider burnishing during drive build |
-
1978
- 1978-08-19 JP JP10124778A patent/JPS5528554A/en active Pending
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS59107428A (en) * | 1982-12-10 | 1984-06-21 | Seiko Epson Corp | Formation of lubricating layer for magnetic recording medium |
JPH0430084B2 (en) * | 1982-12-10 | 1992-05-20 | ||
US7624496B2 (en) * | 2003-08-29 | 2009-12-01 | Hitachi Global Storage Technologies Netherlands B.V. | Method for efficient slider burnishing during drive build |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS576439A (en) | Magnetic recording medium | |
JPS57133521A (en) | Magnetic recording medium | |
JPS5414711A (en) | Magnetic recording medium | |
JPS5550251A (en) | Magnetic toner for electrostatic image development | |
JPS5668928A (en) | Magnetic recording medium | |
JPS5528554A (en) | Magnetic recording medium | |
JPS5654637A (en) | Magnetic recording medium | |
JPS5528553A (en) | Magnetic recording medium | |
JPS54119904A (en) | Magnetic recording medium | |
JPS5528562A (en) | Magnetic recording medium | |
JPS5528560A (en) | Magnetic recording medium | |
JPS5528561A (en) | Magnetic recording medium | |
JPS5528557A (en) | Magnetic recording medium | |
JPS5528558A (en) | Magnetic recording medium | |
JPS5528555A (en) | Magnetic recording medium | |
JPS5528556A (en) | Magnetic recording medium | |
JPS5584041A (en) | Magnetic recording medium | |
JPS5528559A (en) | Magnetic recording medium | |
JPS5597026A (en) | Magnetic recording medium | |
JPS5671822A (en) | Magnetic recording medium | |
JPS5528507A (en) | Magnetic recording tape | |
JPS5517816A (en) | Magnetic recording media | |
JPS5661033A (en) | Magnetic recording medium | |
JPS55122235A (en) | Magnetic disc coating film | |
JPS5517834A (en) | Magnetic recording media |