ES381397A1 - Improvements in or relating to condensation of metal vapour - Google Patents

Improvements in or relating to condensation of metal vapour

Info

Publication number
ES381397A1
ES381397A1 ES381397A ES381397A ES381397A1 ES 381397 A1 ES381397 A1 ES 381397A1 ES 381397 A ES381397 A ES 381397A ES 381397 A ES381397 A ES 381397A ES 381397 A1 ES381397 A1 ES 381397A1
Authority
ES
Spain
Prior art keywords
impeller
spray
condensation
relating
droplets
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
ES381397A
Other languages
Spanish (es)
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
METALLURG PROCESSES Ltd E
Original Assignee
METALLURG PROCESSES Ltd E
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by METALLURG PROCESSES Ltd E filed Critical METALLURG PROCESSES Ltd E
Publication of ES381397A1 publication Critical patent/ES381397A1/en
Expired legal-status Critical Current

Abstract

An impeller for rotation about a vertical axis and suitable for at least partial immersion in a body of molten lead to cast up a spray of droplets has at least one arm of different length from the other(s). As shown there are two pairs of arms 2, 3 and 4, 5 of unequal lengths the arms slope downwards from a central boss 1 (see Fig. 2, not shown) and have terminal scoops 6, 7, 8, 9. A suitable material is ferritic 3% chromium steel, and dimensions are quoted. The impeller is intended for use in an apparatus for condensing zinc from the vapour of a zinc blast furnace by passing it through a spray of molten lead droplets.
ES381397A 1969-07-04 1970-07-03 Improvements in or relating to condensation of metal vapour Expired ES381397A1 (en)

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
GB33881/69A GB1263165A (en) 1969-07-04 1969-07-04 Improvements in or relating to condensation of metal vapour

Publications (1)

Publication Number Publication Date
ES381397A1 true ES381397A1 (en) 1972-11-16

Family

ID=10358668

Family Applications (1)

Application Number Title Priority Date Filing Date
ES381397A Expired ES381397A1 (en) 1969-07-04 1970-07-03 Improvements in or relating to condensation of metal vapour

Country Status (17)

Country Link
JP (1) JPS4921008B1 (en)
BE (1) BE752759A (en)
BG (1) BG17982A3 (en)
CA (1) CA928953A (en)
CS (1) CS192454B2 (en)
DE (1) DE2032161C3 (en)
ES (1) ES381397A1 (en)
FR (1) FR2073296B1 (en)
GB (1) GB1263165A (en)
HU (1) HU166740B (en)
IE (1) IE34338B1 (en)
IL (1) IL34824A0 (en)
NL (1) NL150164B (en)
PL (1) PL82780B1 (en)
RO (1) RO58750A (en)
ZA (1) ZA704448B (en)
ZM (1) ZM8270A1 (en)

Families Citing this family (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS52141308U (en) * 1976-04-19 1977-10-26
JPS6166249A (en) * 1984-09-06 1986-04-05 Matsushita Electric Ind Co Ltd Magnetic recording and reproducing device
JPS61187150A (en) * 1985-02-15 1986-08-20 Akai Electric Co Ltd Reverse type tape running device
GB8617569D0 (en) * 1986-07-18 1986-08-28 Davidson J F Impellers
JPH01133203U (en) * 1988-02-22 1989-09-11

Also Published As

Publication number Publication date
DE2032161A1 (en) 1971-03-25
FR2073296A1 (en) 1971-10-01
PL82780B1 (en) 1975-10-31
CA928953A (en) 1973-06-26
ZM8270A1 (en) 1971-04-22
NL7009936A (en) 1971-01-06
NL150164B (en) 1976-07-15
BE752759A (en) 1970-12-01
HU166740B (en) 1975-05-28
CS192454B2 (en) 1979-08-31
RO58750A (en) 1976-01-15
GB1263165A (en) 1972-02-09
BG17982A3 (en) 1974-03-05
FR2073296B1 (en) 1974-08-09
DE2032161B2 (en) 1973-03-15
IE34338B1 (en) 1975-04-16
IE34338L (en) 1971-01-04
ZA704448B (en) 1971-03-31
DE2032161C3 (en) 1973-10-04
JPS4921008B1 (en) 1974-05-29
IL34824A0 (en) 1970-08-19

Similar Documents

Publication Publication Date Title
ES381397A1 (en) Improvements in or relating to condensation of metal vapour
GB754180A (en) Atomizing aluminium or aluminium alloys
FR2150591A1 (en) Cooling of molten metal - by addition of particles of the same metal(s) at a considerably lower temp
Omori et al. Effect of Plastic Deformation on the Precipitation of Mg-1. 3 Wt per cent Ce Alloy
SU417517A1 (en)
JPS5269805A (en) Dipping body formolten metal
Tsumuraya et al. Precipitation Process in a Pb-0. 038 Wt per cent As Alloy
Syre Effect of Addition Elements on Various Characteristics of Refractory Metals
ES461726A1 (en) Pouring of molten metal from a teeming vessel
GB348398A (en) Improved device for pouring molten metal into a mould
Dzhaparidze Mechanical and Corrosion Properties of the Steels Kh 14 AG 15(DI-13) and 00 Kh 18 N 20 S 3 D 3 M 3 B(EP 667) Re-Melted by Plasma Arc
Nakamura et al. Effect of the Work-Hardened Region at the Notch Tip on the Brittle Fracture of an Fe-3. 12 per cent Si Steel
HARTZ Contribution to the effect of chemical composition on the properties of cobalt-free, heat resistant alloys(German monograph on Co-free heat resistant austenitic steel alloys precipitation hardening and creep strength properties as function of chemical composition)
Chevrand et al. Processing LD Steels With a View to Guaranteeing Carbon Content
SU705001A1 (en) Alloy for steel alloying
Mukhina et al. Influence of the Phase Composition on the Corrosion Resistance of Mg Alloys
GB658110A (en) Improvements in or relating to the manufacture of steel
Seo et al. Influence of the Alloying Element on the Mechanical Properties of a TRIP Steel
GB1028849A (en) Improvements in and relating to discharging molten metal from furnaces
Tyurin et al. The Deoxidation of Iron by Aluminobarium
Masumoto et al. High-Permeability Alloys'Hardperm' of the Ni-Fe-Nb-Cr System
EKEROT Behaviour of slag inclusions of different composition during hot working conditions(Behavior of nonmetallic inclusions in steel during hot working)
GB804957A (en) Discharging static electricity from fluids
Subramanyam Sponge Iron- a Supplement to Scrap
JPS534709A (en) Lining refractory protection method of molten metal vacuum degas vessel