JPH0958657A - Thermally insulated cup - Google Patents

Thermally insulated cup

Info

Publication number
JPH0958657A
JPH0958657A JP7207166A JP20716695A JPH0958657A JP H0958657 A JPH0958657 A JP H0958657A JP 7207166 A JP7207166 A JP 7207166A JP 20716695 A JP20716695 A JP 20716695A JP H0958657 A JPH0958657 A JP H0958657A
Authority
JP
Japan
Prior art keywords
cup
protective cover
paper
heat insulating
side wall
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP7207166A
Other languages
Japanese (ja)
Inventor
Noriko Morita
紀子 森田
Makoto Igarashi
誠 五十嵐
Nobumasa Yamazaki
紳正 山崎
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Toppan Inc
Original Assignee
Toppan Printing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Toppan Printing Co Ltd filed Critical Toppan Printing Co Ltd
Priority to JP7207166A priority Critical patent/JPH0958657A/en
Publication of JPH0958657A publication Critical patent/JPH0958657A/en
Pending legal-status Critical Current

Abstract

PROBLEM TO BE SOLVED: To separate cups satisfactorily, by making the angle of the inclination of the outside of a protective cover and the angle of the inclination of the inside of the main body of each cup different from each other, and by allowing, when superimposing the cups, the contact of the lower end of the outside of the upper cup with the inside of the lower cup. SOLUTION: The main body of a cup has a side wall 14, made of paper, formed as a cylinder of an inverted-truncated-conical shape and a bottom wall 16 closing the vicinity of its small-diameter end. A protective cover 20 having an inverted-truncated-conical shape is disposed so as to cover the entire outside of the side wall 14 of the main body of the cup. This protective cover 20 is formed into a taper structure where its thickness gradually decreases upward. In the taper structure, when the two cups 10 are superimposed one on top of the other, a gap is made between the outside of the upper cup 10 and the inside of the lower cup 10, because the angle of the inclination of the outside of the protective cover 20 is smaller than that of the inside of the main body of the cup. Therefore, a static friction force which occurs between the cups 10 is small, and the upper cup can be pulled from the lower one with a small force.

Description

【発明の詳細な説明】Detailed Description of the Invention

【0001】[0001]

【発明の属する技術分野】本発明は保護カバーがカップ
本体に貼着された断熱カップに関し、特に、内容物に熱
湯を注いで喫食に供する所謂インスタント食品や飲料用
の断熱カップに関する。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a heat insulating cup having a protective cover attached to the cup body, and more particularly to a heat insulating cup for so-called instant foods and beverages in which hot water is poured into the contents for consumption.

【0002】[0002]

【従来の技術】紙製のカップ本体の周囲を断熱構造の紙
製の保護カバーで覆ったものが知られている。この様に
して構成されたカップは、廃棄時の処理が容易であると
共に必要であれば材料の再利用を図ることも可能である
という利点を有する。保護カバーの一例は、カップ本体
の側壁に貼着されたエンボス紙とライナー紙との層構造
からなる。このような断熱カップは、例えば、実開平6
−39717に開示される。
2. Description of the Related Art It is known that a paper cup main body is covered with a paper protective cover having a heat insulating structure. The cup configured in this way has the advantage that it is easy to dispose of when it is discarded and the material can be reused if necessary. An example of the protective cover has a layered structure of embossed paper and liner paper attached to the side wall of the cup body. Such a heat insulating cup is, for example, an actual open flat 6
-39717.

【0003】[0003]

【発明が解決しようとする課題】カップ本体が保護カバ
ーにより覆われてなる断熱カップは、しかし、保護カバ
ーの有する弾力性に起因し、カップどうしを重ねた場合
の結合力が高い。例えば、この種の断熱カップは、内容
物を充填する前は、重ねられた状態で輸送及び貯蔵時さ
れる。従って、この状態から自動供給装置によりカップ
を1つずつ送ろうとした場合に、上側のカップの外面と
下側カップの内面とが完全に面接触するため、カップ離
れの問題が生じる。本発明は上述のような従来の問題点
に鑑みてなされたものであり、カップ離れが良好な断熱
カップを提供することを目的とする。
However, the heat insulating cup in which the cup body is covered with the protective cover has a high binding force when the cups are stacked due to the elasticity of the protective cover. For example, insulating cups of this kind are transported and stored in a stacked state before being filled with the contents. Therefore, when trying to feed the cups one by one from this state by the automatic feeder, the outer surface of the upper cup and the inner surface of the lower cup are completely in surface contact with each other, which causes a problem of cup separation. The present invention has been made in view of the above-mentioned conventional problems, and an object of the present invention is to provide a heat insulating cup with a good cup separation.

【0004】[0004]

【課題を解決するための手段】本発明の第1の視点によ
る断熱カップは、紙製の側壁及び紙製の底壁を有する逆
円錐台型のカップ本体と、前記側壁を覆い且つこれに貼
着された紙製の逆円錐台型の保護カバーと、を具備する
断熱カップにおいて、当該断熱カップの底面と前記保護
カバーの外面とのなす内角が、前記底面と前記カップ本
体の前記側壁の内面とがなす内角よりも小さくなるよう
に、前記保護カバーの厚さが上方に向かって減少し、こ
こで、当該断熱カップを2つ重ねた場合、上側の断熱カ
ップの外面の下端が、下側の断熱カップの内面に対して
当接することを特徴とする。
According to a first aspect of the present invention, there is provided a heat insulating cup, which is an inverted truncated cone type cup body having a paper side wall and a paper bottom wall, and which covers and sticks to the side wall. In a heat insulating cup provided with a paper-made inverted frustoconical protective cover, an inner angle formed between the bottom surface of the heat insulating cup and the outer surface of the protective cover is the bottom surface and the inner surface of the side wall of the cup body. The thickness of the protective cover decreases upward so as to become smaller than the inner angle formed by, and when two heat insulating cups are stacked, the lower end of the outer surface of the upper heat insulating cup is Is abutted against the inner surface of the heat insulating cup.

【0005】本発明の第2の視点による断熱カップは、
本発明の第1の視点による断熱カップにおいて、前記保
護カバーが互いに貼着されたエンボス紙とライナー紙と
を具備し、前記エンボス紙のエンボスの高さの変化によ
り、前記保護カバーの厚さが上方に向かって減少するこ
とを特徴とする。
The heat insulating cup according to the second aspect of the present invention comprises:
In the heat insulating cup according to the first aspect of the present invention, the protective cover comprises embossed paper and liner paper adhered to each other, and the thickness of the protective cover changes according to a change in embossing height of the embossed paper. It is characterized by decreasing upward.

【0006】本発明に係る断熱カップによれば、保護カ
バーの外面の傾斜角とカップ本体の内面の傾斜角との相
違により、カップどうしを重ねた場合でも、上下のカッ
プの外内面が全体に亘って密着しない。このため、上下
のカップ間に生じる静摩擦力は小さく、上側カップを下
側のカップから、小さな力で引抜くことができる。ま
た、保護カバーの上端の厚さが小さいため、実質的なフ
ランジ部の張出し長さを大きくすることができる。
According to the heat insulating cup of the present invention, the outer and inner surfaces of the upper and lower cups are wholly covered even when the cups are stacked due to the difference between the outer surface of the protective cover and the inner surface of the cup body. Does not adhere to each other. Therefore, the static frictional force generated between the upper and lower cups is small, and the upper cup can be pulled out from the lower cup with a small force. Further, since the thickness of the upper end of the protective cover is small, the substantial overhanging length of the flange portion can be increased.

【0007】[0007]

【発明の実施の形態】以下、図面を参照して本発明の実
施の形態を説明する。図1は本発明の実施の形態に係る
断熱カップ10を示す正面図であり、図2は図1図示の
断熱カップの部分切欠斜視図である。
Embodiments of the present invention will be described below with reference to the drawings. 1 is a front view showing a heat insulating cup 10 according to an embodiment of the present invention, and FIG. 2 is a partially cutaway perspective view of the heat insulating cup shown in FIG.

【0008】カップ本体12は、逆円錐台形の筒として
形成された紙製の側壁14と、側壁14の小径端近傍を
閉鎖する底壁16とを有する。側壁14は1枚の板紙を
逆円錐台形に丸め、両側方端部15を重ね合わせて貼着
することにより形成される。底壁16は浅い筒形を脚部
を有し、逆円錐台形の側壁14の下端に嵌め込まれる。
側壁14の小径端即ち下端の周縁は、底壁16の脚部を
包むように内方に折返され、これによりシール性が確保
される。
The cup body 12 has a side wall 14 made of paper formed as an inverted frustoconical cylinder, and a bottom wall 16 closing the vicinity of the small diameter end of the side wall 14. The side wall 14 is formed by rolling a sheet of paperboard into an inverted frustoconical shape and laminating both side end portions 15 on each other. The bottom wall 16 has a shallow tubular shape with legs, and is fitted into the lower end of the inverted truncated cone side wall 14.
The small-diameter end, that is, the peripheral edge of the lower end of the side wall 14 is folded back inward so as to wrap around the leg portion of the bottom wall 16, thereby ensuring the sealing property.

【0009】側壁14の大径端即ち開口端の周縁は外方
に折返されてフランジ部18が形成される。フランジ部
18はカップ本体12を補強すると共に、シート状の蓋
(図示せず)を貼り付けるために使用される。蓋はカッ
プ本体12内に内容物が充填された後に貼り付けられ
る。シート状の蓋に代え、透明な樹脂の成形体等からな
るキャップ(図示せず)をフランジ部18に装着するこ
ともできる。
A large-diameter end of the side wall 14, that is, a peripheral edge of the opening end is folded back outward to form a flange portion 18. The flange portion 18 is used to reinforce the cup body 12 and to attach a sheet-like lid (not shown). The lid is attached after the cup body 12 is filled with the contents. Instead of the sheet-like lid, a cap (not shown) made of a transparent resin molding or the like may be attached to the flange portion 18.

【0010】カップ本体12の側面周囲即ち側壁14の
外面の実質的に全体を覆うように逆円錐台形の保護カバ
ー20が配設される。保護カバー20は、側壁14の外
面全体を覆うように貼着されたエンボス紙24と、エン
ボス紙24の全体を覆うように貼着されたライナー紙2
8と、からなる多層構造をなす。また、保護カバー20
は、その厚さが上方に向かって漸次減少するようなテー
パー構造に形成される。保護カバー20のテーパー構造
は本発明の要部であり、従って、後に詳述する。
An inverted frustoconical protective cover 20 is provided so as to cover substantially the entire side surface of the cup body 12, that is, the outer surface of the side wall 14. The protective cover 20 includes an embossed paper 24 attached to cover the entire outer surface of the side wall 14 and a liner paper 2 attached to cover the entire embossed paper 24.
8 to form a multilayer structure. In addition, the protective cover 20
Is formed in a tapered structure such that its thickness gradually decreases upward. The taper structure of the protective cover 20 is an essential part of the present invention, and will therefore be described in detail later.

【0011】カップ本体12の側壁14及び底壁16を
構成する板紙は、白色の上質紙からなり、その坪量は約
210g/m2 、厚さが約280μmである。側壁14
及び底壁16を構成する板紙の内面には、厚さ約45μ
mのポリエチレン膜13がコーティングされる。側壁1
4用の板紙は、坪量が170g/m2 〜310g/m
2 、厚さが220μm〜420μmに設定される。ま
た、ポリエチレン膜13の厚さは20μm〜60μmに
設定される。
The paperboard forming the side wall 14 and the bottom wall 16 of the cup body 12 is made of white high-quality paper, and has a basis weight of about 210 g / m 2 and a thickness of about 280 μm. Side wall 14
And the inner surface of the paper board that constitutes the bottom wall 16 has a thickness of about 45 μm.
m polyethylene film 13 is coated. Side wall 1
Paperboard for 4 has a basis weight of 170 g / m 2 to 310 g / m
2. The thickness is set to 220 μm to 420 μm. The thickness of the polyethylene film 13 is set to 20 μm to 60 μm.

【0012】エンボス紙24は白色の晒クラフト紙から
なり、その坪量は120g/m2 である。本実施の形態
において、エンボス紙24の全体には、等間隔に配置さ
れた多数の縦溝38と、等間隔に配設された複数の横溝
39とにより区画された多数の縦長の凸部からなるエン
ボス25が形成される(図5参照)。
The embossed paper 24 is made of white bleached kraft paper and has a basis weight of 120 g / m 2 . In the present embodiment, the entire embossed paper 24 has a plurality of vertically long convex portions defined by a plurality of vertical grooves 38 arranged at equal intervals and a plurality of horizontal grooves 39 arranged at equal intervals. The embossing 25 is formed (see FIG. 5).

【0013】エンボス紙24は、エンボス25が通常の
使用によっては潰れない程度の強度を有する一方、加工
が容易であることが必要となる。この観点から、エンボ
ス紙24の坪量の望ましい範囲は、50/m2 〜180
g/m2 である。なお、晒クラフト紙のように繊維長が
大きい紙は、エンボスを形成した際に穴があきにくいと
いう利点を有する。
The embossed paper 24 needs to be easy to process, while the embossed paper 25 has such strength that the embossed paper 25 does not collapse under normal use. From this viewpoint, the desirable range of the basis weight of the embossed paper 24 is 50 / m 2 to 180.
g / m 2 . Note that paper having a large fiber length, such as bleached kraft paper, has an advantage that holes are unlikely to be formed when embossing is formed.

【0014】また、エンボス25は、保護カバー20内
に形成される断熱空気層を実質的に規定する。従って、
エンボス25の形状及び寸法は、当該断熱カップの断熱
性及び保温性の両面を考慮して決定する。エンボス25
として、本実施の形態の模様の他、凹凸点模様、波形模
様等の模様を採用することができる。なお、後述するよ
うに、本実施の形態において、エンボス25の高さは、
保護カバー20の下部、中間部及び上部間で異なり、こ
れにより保護カバー20の厚さが上方に向かって減少す
る。
The embossing 25 also substantially defines an insulating air layer formed within the protective cover 20. Therefore,
The shape and size of the embossing 25 are determined in consideration of both the heat insulating property and the heat retaining property of the heat insulating cup. Embossed 25
In addition to the pattern of the present embodiment, a pattern such as an uneven dot pattern or a wavy pattern can be adopted. As will be described later, in the present embodiment, the height of the embossing 25 is
It differs between the lower part, the middle part and the upper part of the protective cover 20, which reduces the thickness of the protective cover 20 upwards.

【0015】ライナー紙28の坪量は230g/m2
で、その表側の面にはオフセット印刷若しくはグラビア
印刷により商品に関する文字や図柄が施される。ライナ
ー紙28の坪量の望ましい範囲は、180g/m2 〜2
70g/m2 である。この範囲以上であると剛性が高く
なり過ぎ、保護カバー20の加工性が低下する。この範
囲以下であると剛性及び強度が低下し、エンボス25に
倣った凹凸が表面に生じたり、保護カバー20をカップ
本体12に取付けた後、搬送や貯蔵時に破れやすくな
る。
The basis weight of the liner paper 28 is 230 g / m 2.
Then, on the surface on the front side, characters or designs relating to the product are applied by offset printing or gravure printing. The preferable range of the basis weight of the liner paper 28 is 180 g / m 2 to 2
It is 70 g / m 2 . If it is above this range, the rigidity becomes too high, and the workability of the protective cover 20 deteriorates. If it is less than this range, the rigidity and strength will be reduced, and unevenness following the emboss 25 will occur on the surface, or after the protective cover 20 is attached to the cup body 12, it will be easily broken during transportation or storage.

【0016】カップ本体12、エンボス紙24、及びラ
イナー紙28の各部材間は合成糊、例えば酢酸ビニル系
糊、エチレン酢酸ビニル(EVA)系糊により夫々貼着
される。糊としては、この他、種々の公知の糊を使用す
ることができる。例えば、デンプン系糊も使用できる
が、この場合、ライナー紙28の表面にエンボス25に
倣った凹凸が生じやすい。従って、上記の酢酸ビニル系
糊、エチレン酢酸ビニル系糊を使用することが望まし
い。
The members of the cup body 12, the embossed paper 24, and the liner paper 28 are adhered to each other with a synthetic glue, for example, vinyl acetate glue or ethylene vinyl acetate (EVA) glue. In addition to this, various known pastes can be used as the paste. For example, a starch-based glue can be used, but in this case, the surface of the liner paper 28 is likely to have irregularities following the embossing 25. Therefore, it is desirable to use the above vinyl acetate-based glue or ethylene vinyl acetate-based glue.

【0017】次に、保護カバー20のテーパー構造につ
いて詳述する。図1図示の如く、保護カバー20は、そ
の厚さが上方に向かって漸次減少するように形成され
る。例えば、図3図示の如く、保護カバー20の下端の
厚さT1が1.5mm〜2.0mmであると、上端の厚
さT2が0.7mm〜1.0mmというように、上端は
下端の約半分の厚さに設定される。この結果、断熱カッ
プ10の底面と保護カバー20の外面とのなす内角(傾
斜角)が、同底面とカップ本体12の側壁14の内面と
のなす内角(傾斜角)よりも小さくなる。
Next, the taper structure of the protective cover 20 will be described in detail. As shown in FIG. 1, the protective cover 20 is formed such that its thickness gradually decreases upward. For example, as shown in FIG. 3, when the thickness T1 of the lower end of the protective cover 20 is 1.5 mm to 2.0 mm, the thickness T2 of the upper end is 0.7 mm to 1.0 mm. The thickness is set to about half. As a result, the inner angle (tilt angle) formed between the bottom surface of the heat insulating cup 10 and the outer surface of the protective cover 20 is smaller than the inner angle (tilt angle) formed between the bottom surface and the inner surface of the side wall 14 of the cup body 12.

【0018】保護カバー20のテーパー構造は、カップ
どうしを重ねた場合のカップ離れを向上させることを意
図する。例えば、図4図示の如く、本実施の形態に係る
2つのカップ10a、10bを重ねた場合、上側のカッ
プ10bの下端の外径と下側のカップ10aの内径とが
概ね一致する位置で、上側カップ10bの外面の下端が
下側のカップ10aの内面に当接する。この当接状態に
おいて、保護カバー20の外面の傾斜角がカップ本体1
2の内面の傾斜角よりも小さいため、上側のカップ10
bの下端以外の位置では、上側のカップ10bの外面と
下側のカップ10aの内面との間には隙間が生じる。こ
のため、両カップ10a、10b間に生じる静摩擦力は
小さく、上側カップ10bを下側のカップ10aから、
小さな力で引抜くことができる。
The taper structure of the protective cover 20 is intended to improve the cup separation when the cups are stacked. For example, as shown in FIG. 4, when the two cups 10a and 10b according to the present embodiment are stacked, the outer diameter of the lower end of the upper cup 10b and the inner diameter of the lower cup 10a substantially match, The lower end of the outer surface of the upper cup 10b contacts the inner surface of the lower cup 10a. In this abutting state, the inclination angle of the outer surface of the protective cover 20 is changed to the cup body 1
2 is smaller than the inclination angle of the inner surface, the upper cup 10
At positions other than the lower end of b, there is a gap between the outer surface of the upper cup 10b and the inner surface of the lower cup 10a. Therefore, the static frictional force generated between both cups 10a and 10b is small, and the upper cup 10b from the lower cup 10a is
Can be pulled out with a small force.

【0019】保護カバー20のテーパー構造を形成する
ため、本実施の形態においては、図5図示の如く、保護
カバー20が、3つの扇形の領域、即ち下部33、中間
部34及び上部35に区分され、各部ごとにエンボス2
5の高さが異なる。このような構造は、全体が均一な高
さのエンボス25を、各部ごとに適宜な量だけ潰すこと
により得ることができる。エンボス25を潰す作業は、
図5図示の保護カバー20用の成形ブランク32を原料
シートから打ち抜き切断する際に同時に行うことができ
る。この時、エンボス紙24よりライナー紙28の方が
強度が高いため、エンボス紙24のみが潰れる。なお、
エンボス25の高さが3段階であっても、保護カバー2
0外側のライナー紙28が適当な剛性を有するため、カ
ップ本体12に保護カバー20を貼着した後は、保護カ
バー20の厚さは上方に向かって漸次減少するような態
様となる。
In order to form the taper structure of the protective cover 20, in the present embodiment, as shown in FIG. 5, the protective cover 20 is divided into three fan-shaped regions, that is, a lower portion 33, an intermediate portion 34 and an upper portion 35. Embossed 2 for each part
The height of 5 is different. Such a structure can be obtained by crushing the embossing 25 having a uniform height as a whole by an appropriate amount for each part. To crush the emboss 25,
This can be performed simultaneously with punching and cutting the forming blank 32 for the protective cover 20 shown in FIG. 5 from the raw material sheet. At this time, since the liner paper 28 is stronger than the embossed paper 24, only the embossed paper 24 is crushed. In addition,
Even if the height of the embossing 25 is three levels, the protective cover 2
Since the outermost liner paper 28 has an appropriate rigidity, the thickness of the protective cover 20 gradually decreases upward after the protective cover 20 is attached to the cup body 12.

【0020】上述の如く本実施の形態に係る断熱カップ
によれば、カップどうしを重ねた場合でも、保護カバー
20のテーパー構造により、上側のカップの外面の下端
のみが、下側のカップの内面に対して当接し、上下のカ
ップの外内面が全体に亘って密着することがなくなる。
従って、保護カバー20が有する高い弾力性にもかかわ
らず、カップ離れが良好となる。
As described above, according to the heat insulating cup of the present embodiment, even when the cups are stacked on top of each other, the tapered structure of the protective cover 20 causes only the lower end of the outer surface of the upper cup to be the inner surface of the lower cup. The outer and inner surfaces of the upper and lower cups do not come into close contact with each other.
Therefore, despite the high elasticity of the protective cover 20, the cup separation is good.

【0021】また、保護カバー20の上端の厚さが小さ
いため、図3図示の如く、保護カバー20の上端外面か
らカップ本体12のフランジ部18の先端までの長Lさ
が従来の構造に比べ大きくなる。即ち、実質的なフラン
ジ部18の張出し長さが大きくなる。このため、搬送装
置のコンベアホルダからの脱落が防止されると共に、フ
ランジ部18にシート状の蓋(図示せず)を貼り付ける
際に、押圧作用面積が大きくとれるため、広いシール幅
を形成することが可能となる。
Since the thickness of the upper end of the protective cover 20 is small, the length L from the outer surface of the upper end of the protective cover 20 to the tip of the flange portion 18 of the cup body 12 is smaller than that of the conventional structure as shown in FIG. growing. That is, the substantial overhanging length of the flange portion 18 increases. For this reason, it is possible to prevent the carrier device from falling off the conveyor holder, and when a sheet-like lid (not shown) is attached to the flange portion 18, a large pressing action area can be taken, so that a wide seal width is formed. It becomes possible.

【0022】次に、本発明の実施の形態に係る断熱カッ
プの製造方法について説明する。先ず、公知のカップ成
形装置によりカップ本体12を形成する。ここで、先
ず、逆円錐台形に丸められた側壁14と浅い筒形状の底
壁16とを組合わせ、カップ本体12の原型を形成す
る。次に、カップ本体12の開口端周縁において側壁1
4を外方に折返してフランジ部18を形成する。
Next, a method of manufacturing the heat insulating cup according to the embodiment of the present invention will be described. First, the cup body 12 is formed by a known cup molding device. Here, first, the side wall 14 rounded in the shape of an inverted truncated cone and the bottom wall 16 having a shallow cylindrical shape are combined to form a prototype of the cup body 12. Next, at the peripheral edge of the opening end of the cup body 12, the side wall 1
4 is turned outward to form the flange portion 18.

【0023】一方、公知の打ち抜き装置において、保護
カバー20の成形ブランクを形成する。このため、先
ず、エンボス紙24の原料シート、例えばコルゲート紙
のシートとライナー紙28の原料シートとを貼着する。
ライナー紙28の原料シートの表面には、オフセット印
刷或いはグラビア印刷により印刷を行う。この印刷によ
り、多数枚の保護カバー20に対応する、商品に関する
文字や図柄がライナー紙28の原料シートの表面に施さ
れる。
On the other hand, a molding blank of the protective cover 20 is formed in a known punching device. Therefore, first, a raw material sheet of the embossed paper 24, for example, a corrugated paper sheet and a raw material sheet of the liner paper 28 are attached.
Printing is performed on the surface of the raw material sheet of the liner paper 28 by offset printing or gravure printing. By this printing, the characters and designs related to the products corresponding to the large number of protective covers 20 are applied to the surface of the raw material sheet of the liner paper 28.

【0024】次に、貼着されたエンボス紙24及びライ
ナー紙28の原料シートを、ライナー紙28上の文字や
図柄に合わせて順次打抜き切断する。これにより、カッ
プ本体12の側面周囲の寸法に適合した寸法を有する扇
形の保護カバー20の成形ブランク32を得ることがで
きる。
Next, the material sheets of the embossed paper 24 and the liner paper 28 that have been adhered are sequentially punched and cut according to the characters and designs on the liner paper 28. As a result, it is possible to obtain the molding blank 32 of the fan-shaped protective cover 20 having a size adapted to the size around the side surface of the cup body 12.

【0025】成形ブランクの打ち抜き切断の際、保護カ
バー20のテーパー構造を得るため、上述の如く、エン
ボス25を、図5図示の下部33、中間部34及び上部
35ごとに異なる量で潰す。このため、例えば、打ち抜
き用の切断刃と共に、下部33、中間部34及び上部3
5ごとに堅さの異なるゴム製プレス部材を使用すること
ができる。なお、下部33についてはエンボス25を全
く潰さなくともよい。
In punching and cutting the molding blank, in order to obtain the taper structure of the protective cover 20, the embossing 25 is crushed by different amounts for the lower portion 33, the intermediate portion 34 and the upper portion 35 shown in FIG. 5, as described above. Therefore, for example, together with the cutting blade for punching, the lower portion 33, the intermediate portion 34, and the upper portion 3
It is possible to use a rubber press member having different hardness for each 5. The lower portion 33 does not need to have the embossed 25 crushed at all.

【0026】また、成形ブランクの打ち抜き切断の際、
エンボス紙24の原料であるコルゲート紙の縦溝38と
交差するように、罫線ブレードにより横溝39をプレス
する。これにより、縦溝38と横溝39とにより区画さ
れた多数の縦長の凸部からなるエンボス25が形成され
る。この様なエンボス25を形成することにより、コル
ゲート紙をそのまま使用した場合に比べて、保護カバー
20を組立てる際の作業性及び確実性を向上させること
ができる。なお、横溝39の形成は、エンボス紙24の
原料シートとなるコルゲート紙のシートとライナー紙2
8の原料シートとの貼着後であれば、成形ブランクの打
ち抜き前でも行うことができる。
When punching and cutting the molding blank,
The lateral groove 39 is pressed by a ruled blade so as to intersect the vertical groove 38 of the corrugated paper, which is the raw material of the embossed paper 24. As a result, the embossment 25 is formed of a large number of vertically elongated protrusions defined by the vertical groove 38 and the horizontal groove 39. By forming such an emboss 25, it is possible to improve workability and certainty when assembling the protective cover 20, as compared with the case where the corrugated paper is used as it is. The formation of the lateral groove 39 is performed by forming the corrugated sheet and the liner sheet 2 which are the raw material sheets of the embossed sheet 24.
It can be carried out before the molding blank is punched as long as it is adhered to the raw material sheet of No. 8.

【0027】次に、保護カバー20をカップ本体12の
側壁14に貼着する。これは、例えば、巻付け装置によ
り、保護カバー20をカップ本体12の側面周囲に巻付
けながら糊によって貼着することにより行うことができ
る。この巻付け方法を採用した場合には、保護カバー2
0は、その両側方端部を、重合わせることなく、突き合
わせた状態でカップ本体12に装着することができる。
Next, the protective cover 20 is attached to the side wall 14 of the cup body 12. This can be performed, for example, by wrapping the protective cover 20 around the side surface of the cup body 12 with a wrapping device and adhering it with glue. When this winding method is adopted, the protective cover 2
0 can be attached to the cup main body 12 in a state of being abutted with each other without overlapping the both ends.

【0028】また、保護カバー20を巻付ける方法に代
え、予め保護カバー20だけでカップ本体12の側壁1
4と概ね同じ逆円錐台形の筒に組立て、その後、保護カ
バー20をカップ本体12に嵌め込みながら貼着する方
法を採用することもできる。この場合、保護カバー20
の成形ブランクには一側方端部に糊代が付設され、保護
カバー20は、両側方端部を重合わせた状態で形成され
ることとなる。
Further, instead of the method of winding the protective cover 20, the side wall 1 of the cup body 12 is previously prepared only by the protective cover 20.
It is also possible to adopt a method of assembling into a cylinder having an inverted truncated cone shape which is substantially the same as that of No. 4, and then attaching the protective cover 20 while fitting it into the cup body 12. In this case, the protective cover 20
The molding blank is provided with a glue margin at one side end, and the protective cover 20 is formed in a state where both side ends are overlapped.

【0029】[0029]

【発明の効果】本発明に係る断熱カップによれば、保護
カバーがテーパー構造となっているため、カップどうし
を重ねた場合でも、上下のカップの外内面が全体に亘っ
て密着することがなくなる。このため、保護カバーが有
する高い弾力性にもかかわらず、カップ離れが良好とな
る。また、保護カバーの上端の厚さが小さいため、実質
的なフランジ部の張出し長さを大きくすることができ
る。
According to the heat insulating cup of the present invention, since the protective cover has the taper structure, the outer and inner surfaces of the upper and lower cups do not adhere to each other even when the cups are stacked. . Therefore, the cup separation is good despite the high elasticity of the protective cover. Further, since the thickness of the upper end of the protective cover is small, the substantial overhanging length of the flange portion can be increased.

【図面の簡単な説明】[Brief description of drawings]

【図1】本発明の実施の形態に係る断熱カップを示す正
面図。
FIG. 1 is a front view showing a heat insulating cup according to an embodiment of the present invention.

【図2】図1図示の断熱カップの部分切欠斜視図。2 is a partially cutaway perspective view of the heat insulating cup shown in FIG. 1. FIG.

【図3】図1図示の断熱カップのカップ本体と保護カバ
ーとの関係を拡大して示す図。
3 is an enlarged view showing a relationship between a cup body and a protective cover of the heat insulating cup shown in FIG.

【図4】図1図示の断熱カップどうしを重ねた状態を示
す概略図。
FIG. 4 is a schematic view showing a state in which the heat insulating cups shown in FIG. 1 are stacked.

【図5】図1図示の断熱カップの保護カバー用の成形ブ
ランクを、エンボス紙側から見た状態で示す平面図。
5 is a plan view showing a molding blank for the protective cover of the heat insulating cup shown in FIG. 1 as viewed from the embossed paper side.

【符号の説明】[Explanation of symbols]

10…断熱カップ、12…カップ本体、14…側壁、1
6…底壁、18…フランジ部、20…保護カバー、24
…エンボス紙、25…エンボス、28…ライナー紙、3
2…成形ブランク、38…縦溝、39…横溝。
10 ... Insulation cup, 12 ... Cup body, 14 ... Side wall, 1
6 ... Bottom wall, 18 ... Flange part, 20 ... Protective cover, 24
... embossed paper, 25 ... embossed, 28 ... liner paper, 3
2 ... Molding blank, 38 ... Vertical groove, 39 ... Horizontal groove.

Claims (2)

【特許請求の範囲】[Claims] 【請求項1】紙製の側壁及び紙製の底壁を有する逆円錐
台型のカップ本体と、前記側壁を覆い且つこれに貼着さ
れた紙製の逆円錐台型の保護カバーと、を具備する断熱
カップにおいて、 当該断熱カップの底面と前記保護カバーの外面とのなす
内角が、前記底面と前記カップ本体の前記側壁の内面と
がなす内角よりも小さくなるように、前記保護カバーの
厚さが上方に向かって減少し、ここで、当該断熱カップ
を2つ重ねた場合、上側の断熱カップの外面の下端が、
下側の断熱カップの内面に対して当接することを特徴と
する断熱カップ。
1. A reverse frustoconical cup body having a paper side wall and a paper bottom wall, and a paper reverse frustoconical protection cover that covers the side wall and is attached to the cup side wall. In the heat insulating cup, the thickness of the protective cover is set so that the inner angle formed by the bottom surface of the heat insulating cup and the outer surface of the protective cover is smaller than the inner angle formed by the bottom surface and the inner surface of the side wall of the cup body. Decreases upward, and when two heat insulating cups are stacked, the lower end of the outer surface of the upper heat insulating cup is
An adiabatic cup characterized by being in contact with the inner surface of a lower adiabatic cup.
【請求項2】前記保護カバーが互いに貼着されたエンボ
ス紙とライナー紙とを具備し、前記エンボス紙のエンボ
スの高さの変化により、前記保護カバーの厚さが上方に
向かって減少することを特徴とする請求項1記載の断熱
カップ。
2. The protective cover comprises embossed paper and liner paper adhered to each other, and the thickness of the protective cover decreases upward due to a change in embossing height of the embossed paper. The heat insulating cup according to claim 1, wherein:
JP7207166A 1995-08-14 1995-08-14 Thermally insulated cup Pending JPH0958657A (en)