CN105330625A - Method for preparing furfural by adopting high-temperature pressurizing pretreatment - Google Patents

Method for preparing furfural by adopting high-temperature pressurizing pretreatment Download PDF

Info

Publication number
CN105330625A
CN105330625A CN201510820337.1A CN201510820337A CN105330625A CN 105330625 A CN105330625 A CN 105330625A CN 201510820337 A CN201510820337 A CN 201510820337A CN 105330625 A CN105330625 A CN 105330625A
Authority
CN
China
Prior art keywords
furfural
temperature pressurizing
adopting high
liquid
treatment
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510820337.1A
Other languages
Chinese (zh)
Inventor
达力
达兴
蒋超
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
CHUZHOU RUNDA SOLVENTS CO LTD
Original Assignee
CHUZHOU RUNDA SOLVENTS CO LTD
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CHUZHOU RUNDA SOLVENTS CO LTD filed Critical CHUZHOU RUNDA SOLVENTS CO LTD
Priority to CN201510820337.1A priority Critical patent/CN105330625A/en
Publication of CN105330625A publication Critical patent/CN105330625A/en
Pending legal-status Critical Current

Abstract

The invention provides a method for preparing furfural by adopting high-temperature pressurizing pretreatment. The method comprises the following steps: step one, collecting crop raw materials; step two, chopping the collected raw materials; step three, adding water, mixing the materials in a ratio of solids to liquids being 1:1, then performing high-temperature pressurizing treatment with a pressure cooker, and performing hydrolysis under the action of diluted acid to obtain a furfural-containing liquid; step four, crystalizing the liquid and finishing processing production. According to the method for preparing the furfural by adopting high-temperature pressurizing pretreatment, a high-temperature pressurizing mode is adopted to treat corresponding crop fiber, so that redundant hemicellulose and lignin in the materials are reduced remarkably, and the furfural yield is increased.

Description

A kind of method adopting high-temperature pressurizing pre-treatment to prepare furfural
Technical field
The present invention relates to furfural preparation field, particularly a kind of method adopting high-temperature pressurizing pre-treatment to prepare furfural.
Background technology
The agricultural byproducts of the furfural industrially luxuriant sugar of the many contractings of multiplex carbohydrate containing are raw material, are hydrolyzed under the effect of diluted acid, and further water ringization manufactures furfural.Furfural is excellent solvent, also for the preparation of medicine and Industrial products.Can be used to produce furans, polyamide fibre 66 and coromegine etc., few fibers just can carry out furfural processing after needing to carry out pre-treatment, and not so its interior half fiber or xylogen are often too much, can affect aldehyde rate.
Summary of the invention
For above problem, the present invention is a kind of method adopting high-temperature pressurizing pre-treatment to prepare furfural, high-temperature pressurizing mode is adopted to process corresponding plant fiber, thus significantly by half fiber unnecessary in its material and xylogen, and then improve furfural productive rate, for reaching this object, the invention provides a kind of method adopting high-temperature pressurizing pre-treatment to prepare furfural, it is characterized in that, comprise the following steps:
The first step, to collect as raw material;
Second step, the raw material gathered carried out chopping process;
3rd step, add water and mix by solid-liquid 1:1, then carry out high-temperature pressurizing process by pressure kettle, then be hydrolyzed under the effect of diluted acid, obtain the liquid containing furfural;
4th step, crystallization treatment is carried out to liquid, complete processing.
The present invention is a kind of method adopting high-temperature pressurizing pre-treatment to prepare furfural, high-temperature pressurizing mode is adopted to process plant fiber, half fiber or xylogen in crop significantly can be reduced after adopting pressure kettle, and then can significantly reduce fibrous polymer degree, thus significantly improve product go out aldehyde rate.
Embodiment
The present invention is a kind of method adopting high-temperature pressurizing pre-treatment to prepare furfural, adopts high-temperature pressurizing mode to process corresponding plant fiber, thus significantly by half fiber unnecessary in its material and xylogen, and then improve furfural productive rate.
Adopt high-temperature pressurizing pre-treatment to prepare a method for furfural, it is characterized in that, comprise the following steps:
The first step, to collect as raw material;
Second step, the raw material gathered carried out chopping process;
3rd step, add water and mix by solid-liquid 1:1, then carry out high-temperature pressurizing process by pressure kettle, then be hydrolyzed under the effect of diluted acid, obtain the liquid containing furfural;
4th step, crystallization treatment is carried out to liquid, complete processing.
The above is only preferred embodiment of the present invention, is not restriction the present invention being made to any other form, and any amendment done according to technical spirit of the present invention or equivalent variations, still belong to the present invention's scope required for protection.

Claims (1)

1. adopt high-temperature pressurizing pre-treatment to prepare a method for furfural, it is characterized in that, comprise the following steps:
The first step, to collect as raw material;
Second step, the raw material gathered carried out chopping process;
3rd step, add water and mix by solid-liquid 1:1, then carry out high-temperature pressurizing process by pressure kettle, then be hydrolyzed under the effect of diluted acid, obtain the liquid containing furfural;
4th step, crystallization treatment is carried out to liquid, complete processing.
CN201510820337.1A 2015-11-24 2015-11-24 Method for preparing furfural by adopting high-temperature pressurizing pretreatment Pending CN105330625A (en)